Postby downunder » Thu Mar 25, 2021 12:26 pm
No,
Not sanding. Use a fine metal wool.
Simply b/c wool will conform to shape and sand paper will just clog.
Steel wool all the way.
-
Jyoder
- Very Frequent Poster
- Posts: 574
- Joined: Thu Jul 20, 2017 8:31 pm
- Kiting since: 2015
- Local Beach: Chesapeake Bay (Annapolis area)
- Gear: Zeeko bullet Foil and DIY board
- Brand Affiliation: None
- Location: Annapolis, Maryland
-
Has thanked:
18 times
-
Been thanked:
168 times
Postby Jyoder » Thu Mar 25, 2021 3:17 pm
Matteo V wrote: ↑Wed Mar 24, 2021 6:50 pm
Jyoder wrote: ↑Wed Mar 24, 2021 5:29 pm
Matteo V wrote: ↑Wed Mar 24, 2021 3:37 pm
That said, I am 99.99% sure your point of failure, especially on a tube, is not going to be glue adhesion at the joint. It's better to just say "screw it" on the proper surface contaminate removal, sand, and slightly over build the joint to compensate.
That’s exactly where my early carbon bars failed as I did not clean the inside of the tube. The tube cracked and broke away from the inner “slug”. Zero failures after I started cleaning the tube.
Metal inside? Thermal expansion can induce stresses in that case.
No metal, just epoxy cylinder, nice and smooth. Release agent works, definitely gotta remove it to get a good bond.
-
Trent hink
- Very Frequent Poster
- Posts: 996
- Joined: Mon Jan 07, 2019 4:59 am
- Kiting since: 1998
- Weight: 83 kg.
- Local Beach: Nokomis beach, Turtle beach, Venice inlet, lido key
- Style: Creepy old man
- Gear: Peak4, LF, solo, Moses 633 hydrofoil, couple of surfboards, a twintip I made in 2008.
- Brand Affiliation: once made an attempt to manufacture and market "Anomaly" twin-tip boards.
-
Has thanked:
296 times
-
Been thanked:
250 times
Postby Trent hink » Thu Mar 25, 2021 4:47 pm
Steel wool is coated with oil, I would not use it on a surface I was planning to epoxy.
-
downunder
- Very Frequent Poster
- Posts: 2814
- Joined: Mon Jul 01, 2013 7:16 am
- Gear: building my own
- Brand Affiliation: None
- Location: Perth, Australia
-
Has thanked:
153 times
-
Been thanked:
160 times
Postby downunder » Fri Mar 26, 2021 1:55 am
Use paint prep solvent after.
Infact, paint prep is needed after anything, correct? Even your fingers will leave oils, if we are that much concerned and pedantic.